I'd better check it works... I need around 1300 degrees C
Weld up a couple of canisters and coat them with white paint - The paint contains titanium dioxide which will prevent the canister welding to the powdered steel.
And add a few stainless steel scouring pads
No pics of teh next bit, but I compress/compact the whole lot down HARD and weld the top on. it goes in teh forge for about 25 mins to fully heat through - the new forge gets hot enough in about 20 mins, and when it comes out the steel is white hot. smashy smashy and fingers crossed...
Result. It's compressed by about 2/3 and appears solid
Time spent prepping everything, getting forge up to temp and removing the canister... about an hour and a half.